Synthesis of the precursors, using research grade materials and locally available facilities, is optimized in order to obtain a suitable sol for BaTiO3. The optimally synthesized BaTiO3 sol is then spun onto Cu substrates to obtain films of thickness ~0.5 μm. The deposited BaTiO3 films are...
Persistent link: https://www.econbiz.de/10005080520
Bayerite sol is spun onto single crystal Si substrate, after synthesis and optimization, to obtain films of thickness ~ 0.2 μm. The deposited films are room temperature dried and then heated up to a temperature of 350°C in order to obtain Al2O3. Surface and structural changes, during heating,...